SouthArk370Z has a reputation beyond reputeSouthArk370Z has a reputation beyond reputeSouthArk370Z has a reputation beyond reputeSouthArk370Z has a reputation beyond reputeSouthArk370Z has a reputation beyond reputeSouthArk370Z has a reputation beyond reputeSouthArk370Z has a reputation beyond reputeSouthArk370Z has a reputation beyond reputeSouthArk370Z has a reputation beyond reputeSouthArk370Z has a reputation beyond reputeSouthArk370Z has a reputation beyond repute
Default

Quote:
Originally Posted by Z_ealot View Post
Thanks everyone for the responses, just had a lot of people telling me they were cast iron cause i had to have an o2 bung welded back on after it broke off while trying to change a bad o2 sensor and everyone was saying to get another manifold cause the weld wouldnt hold cause "the manifolds are cast iron"
With cast iron, brazing works well in most applications. Cast iron is difficult (but not impossible) to weld.
__________________
Steering Lock Links - Search The370Z Bookmarklet - FSM @ NICOclub
Mankind has progressed past the need for war but we haven't evolved that far. - NachoMahma