Mike has a reputation beyond reputeMike has a reputation beyond reputeMike has a reputation beyond reputeMike has a reputation beyond reputeMike has a reputation beyond reputeMike has a reputation beyond reputeMike has a reputation beyond reputeMike has a reputation beyond reputeMike has a reputation beyond reputeMike has a reputation beyond reputeMike has a reputation beyond repute
Default

Quote:
Originally Posted by horty24 View Post
Mike is right, 380-400 degrees for 15-20 minutes will melt them or at least deform them. Plus powder does not work on plastic anyways. It can only be molded into the process.
second part is not quite correct. I've been powdercoating plastic that can handle the temperature for years. I have developed my own process of doing it.





Plastic center cap:
__________________